A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quality of sputtered Si3N4 films
Quality of sputtered Si3N4 films
2005-02-22
amol kumar singh
2005-02-23
Michael D Martin
2005-03-05
Pradeep Dixit
What RGA to buy
2005-03-06
Andrew Xiang
Quality of sputtered Si3N4 films
Pradeep Dixit
2005-03-05
Dear Mr. Martin,

I just seen your reply.

I need to deposit a thin 150 nm Si3N4 layer on a metal pattern Cr. My
lab has Si3N4 furnace, but i can not use furnace as the metal will
contaminate it, we don't have PECVD method for nitride deposition. So
i have only choice to go for sputtering process.

Can you give me some process parameters for Si3N4 sputtering, power,
current substrate temp, deposition rate ??

Do you think, SiO2 sputtering is a good choice than Si3N4 sputtering ?
Is pin hole problem will remain in SiO2 pattern ?

Thanks,
Pradeep

On Wed, 23 Feb 2005 13:58:33 -0500, Michael D Martin
 wrote:
> Hi Amol,
>    Standard sputtering of SixNy is problematic for use in MEMS
> devices. First it has a low sputter yield, so it takes a long time to
> deposite a resonable thickness. Second, and probably most important,
> these films always have lots of pin holes. So I would not count on these
> films for a masking layer.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
University Wafer
MEMS Technology Review