Bosch Conditions for .8 micron pillars
2005-03-08
[email protected]
2005-03-08
Michael D Martin
Bosch Conditions for .8 micron pillars
Michael D Martin
2005-03-08
You might try running dep. and etch gases at the same time, i.e. no
parameter switching. This approach worked for producing 0.8 micron
pillars that were about 5 microns long.

-Mike Martin
 U. of Louisville