A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Bosch process
Bosch process
2005-03-09
Pavel Neuzil
2005-03-10
Kasman , Elina
2005-03-10
Michael D Martin
PECVD PolySi Deposition
2005-03-11
Eric Dy
High fequency amplification
2005-03-11
Vikas Nair
2005-03-11
Isaac Wing Tak Chan
Microscopy for Semiconductor Application
2005-03-13
li cai
2005-03-12
li cai
etch sub-micron holes in PMMA patterned Aluminum
2005-03-12
Xin Heng
Bosch process
Kasman , Elina
2005-03-10
In fact, during Bosch process SF6 and C4F8 are turned on
interchangeably: one is building protective polymer, the other is
etching. Yes, there is also oxygen involved, but I do not remember the
exact recipe.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing