A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: coating a teflon layer on 8um glass spheres
coating a teflon layer on 8um glass spheres
2005-03-17
Yuejun Zhao
help..."stitch" two array together
2005-03-17
[email protected]
SUMMiT product line
2005-03-17
[email protected]
looking for recommendations
2005-03-17
[email protected]
2005-03-19
Natalya
coating a teflon layer on 8um glass spheres
Yuejun Zhao
2005-03-17
Do you have any experience about coating a teflon layer on 8um glass spheres

Now I meet some problems when I am preparing to make a high contact angle
hydrophobic particles in powder. I have some borosilicate glass spheres
(diameter is about 8um) and teflon solution. I make the hydrophilic particles
into the teflon solution and mix them a long time. But when I spray the solutin
on a surface, the particles come together and hardly removal from the surface.
What I want is to get the powdery teflon coating glass spheres, but I think the
method I used could not work.

Do you have some suggestions to me? Which method should I take? Thanks in
advance.

Zhao Yuejun

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer
The Branford Group