Hi there,

I have a Ti(300A)/Al(1400A) on a Si wafer. I am trying to do a lift off using
AZ400K developer because i am using a bi-layer photoresist (LOR 5A and S1813),
but for some reason it seems to me that the developer is attacking or etching
the Al.

Any suggestions on how to solve this problem?


Thank you


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.