MEMSnet Home: MEMS-Talk: Problems with Lift-off
Problems with Lift-off
2005-03-21
Rameez Chatni
2005-03-22
Jesse D Fowler
2005-03-21
Washington, Erika B
2005-03-21
ahajjiah
Problems with Lift-off
Washington, Erika B
2005-03-21
For lift-off, we use Microchem's MP 1165 (SU-8 developer).  It is a
cheaper version of Nano remover PG.  Do not dilute the solution and heat
it to at least 70 deg C.  Lift off may take as long as 20 minutes
depending on the thickness, but it works like a champ and doesn't attack
Al.

-E. Washington

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.