Several causes may lead to defective electroplating you describe including
inadequate adhesion of PR to the seed layer or, the PR is not compatible
with your Au plating solution especially if the solution pH is more
alkaline.
Also, excessive current density may cause gas evolution and subsequent
peeling.

I. Kadija
www.fibrotools.com