Hi all,
We are considering thermal oxidation polishing(oxidize silicon and denude
oxide...), but the temperature can only be 700 degrees because the silicon film
is on a substrate of glass. Does it work under that low temperature? Are there
any other ways to smooth the surface?
I'm looking forward to your reply. Thanks in advance.

Guangbo Li


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation