MEMSnet Home: MEMS-Talk: Hillock formation on Au surface
Hillock formation on Au surface
2005-03-24
Steven McMaster
Hillock formation on Au surface
Steven McMaster
2005-03-24
Using sputtered Ti/Pt/Au (350nm) stack on GaAs devices shows no signs of
hillock formation; however Ti/Pt/Au (1000nm) shows hillocks at the Au
surface. What is the mechanism of this hillock formation and does anyone
know why it is evident using thicker Au films? Even more so, does anyone
know how to avoid them?

Regards,
Steven.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation