Reg: seed layer on a negative resist
2005-03-28
Krishna Vummidi
Reg: seed layer on a negative resist
Krishna Vummidi
2005-03-28
hello,

Im trying to e-beam evaporate/sputter a seed layer on a negative resist. The
thickness of seed layer is around 2000A over patterned photo-resist of thickness
of 1.5 - 2 um. I would then spin, pattern another resist and electroplate
(that's why the seed layer).

My concern is discontinuity of the seed layer on top of the negative resist. Can
anyone suggest how i can deposit a continuous seed layer on top negative resist
by e-beam evaporation. Sputtering might be a easier way out. But Im more
interested in e-beam evaporation.

thanks,
krishna
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
University Wafer
Harrick Plasma, Inc.