A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Plasma etching with sloped sidewalls.
Plasma etching with sloped sidewalls.
2005-03-30
Bruce Altemus
2005-03-30
Isaac Wing Tak Chan
2005-03-30
Shane Arthur McColman
2005-03-30
Bruce Altemus
2005-03-30
Isaac Wing Tak Chan
2005-03-31
Robert Dean
2005-03-31
Wilson, Thomas
2005-04-06
[email protected]
Plasma etching with sloped sidewalls.
Bruce Altemus
2005-03-30
Hello everyone,

I am attempting to generate a sloped side wall with an angle of ~85 degrees
using a fluorine chemistry etching silicon. The mask being used in this
application is Cr. I have seen several papers on a combined bosch but this
has not proved to be successful in my case. I continue to get very nice
anisotropic etching. Thanks for your assistance.

Bruce Altemus


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Nano-Master, Inc.