>Try Aqua Regia. The composition is HCl: HNO3:H20 = 3:1:4
>
>> ----------
>> From:        Andrew CAMPITELLI[SMTP:[email protected]]
>> Reply To:    Andrew CAMPITELLI;[email protected]
>> Sent:        Monday, February 16, 1998 10:54 PM
>> To:  [email protected]
>> Subject:     transparent Au etchant...
>>
>> Dear Colleagues,
>> I am searching for a supplier for a gold etchant that is transparent
>> (clear).
>> We are currently using a KI solution, which works well but has the major
>> disadvantage of being non-transparent.
>> Any suggestions would be greatly appreciated.
>> Thank you.
>> Andrew
>>
>>
>>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
University Wafer
Nano-Master, Inc.