MEMSnet Home: MEMS-Talk: Stripping Off metal
Stripping Off metal
2005-03-30
ahajjiah
2005-03-30
Neal Ricks
Stripping Off metal
Neal Ricks
2005-03-30
The remainder might be Ti-based.  Can you try a Ti etch like 1::3 HNO3 :: H2O2?

ahajjiah  wrote:

I have a Ti/Al metalization on a GaN wafer. I have tried to strip off the
metals by using Aqua Regia (3:1 HCL:HNO3). I left the sample in the acid for 6
hrs. It seems that most of the metals got stripped off, but there are still
some metals on the sample.

Any suggestions on how to remove the metals completely?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.