Hello everyone,

I need to etch 1-2 microns of oxide anisotropically using 1 micron of AZ-4110
photoresist as my mask.  I have a parallel plate RIE with CF4, SF6, Ar, and O2
available.  Could anyone help me with some starting parameters or some
literature?  Thanks for your help.