MEMSnet Home: MEMS-Talk: How to do the lift off process after aluminumdeposition? It is negative resist.
How to do the lift off process after aluminum deposition? It is negative resist.
2005-03-31
Duan
How to do the lift off process after aluminumdeposition? Itis negative resist.
2005-03-31
Jesse D Fowler
microstructured Pt thermal sensor
2005-04-01
Erik Jung
How to do the lift off process after aluminumdeposition? It is negative resist.
2005-03-31
Hongjun-ECE
2005-03-31
Duan
How to do the lift off process afteraluminumdeposition? Itis negative resist.
2005-03-31
Jesse D Fowler
How to do the lift off process afteraluminumdeposition? It is negative resist.
2005-03-31
Hongjun-ECE
How to do the lift off process afteraluminumdeposition? It is negative resist.
2005-03-31
Brent Garber
How to do the lift off process after aluminumdeposition? It is negative resist.
2005-03-31
Shile
How to do the lift off process after aluminumdeposition? It is negative resist.
Hongjun-ECE
2005-03-31
What type of negative resist are you using? If SU8 with the pattern, it is
pretty hard to have a liftoff.

If you just want negative resist without any other requirement, AZ5214 would
be the best. Good luck.

Hongjun Zeng, PhD

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing