MEMSnet Home: MEMS-Talk: microstructured Pt thermal sensor
How to do the lift off process after aluminum deposition? It is negative resist.
2005-03-31
Duan
How to do the lift off process after aluminumdeposition? Itis negative resist.
2005-03-31
Jesse D Fowler
microstructured Pt thermal sensor
2005-04-01
Erik Jung
How to do the lift off process after aluminumdeposition? It is negative resist.
2005-03-31
Hongjun-ECE
2005-03-31
Duan
How to do the lift off process afteraluminumdeposition? Itis negative resist.
2005-03-31
Jesse D Fowler
How to do the lift off process afteraluminumdeposition? It is negative resist.
2005-03-31
Hongjun-ECE
How to do the lift off process afteraluminumdeposition? It is negative resist.
2005-03-31
Brent Garber
How to do the lift off process after aluminumdeposition? It is negative resist.
2005-03-31
Shile
microstructured Pt thermal sensor
Erik Jung
2005-04-01
Dear colleagues,
do you have experience in microstructuring platinum for thermal sensors?
Is there a commercial supplier or an institute doing such sensors?
Range of reliable thermal operation should be -100?C...+200?C and response
time <10ms.
For the application I am doing this inquiry, currently Pt thermal sensor
wires are used.

Regards!

Erik Jung
Fraunhofer IZM
Berlin/Germany

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics