my spin speed is 4000rpm with a ramp of 30000r/s, and the prebake temperature is
100 degree c with a time of 1 minute, but there is always some photoresist
remained no matter how long the develop time, why? Is the pre bake temperature
too high and the the photoresist been destroyed?



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering