RE: Problem in photolithography
2005-04-01
Runkel, Frank
RE: Problem in photolithography
Runkel, Frank
2005-04-01
Dear anonymous mems-talk member

without knowing any details of your photolithography process, it is
difficult to give specific advices. However, you should consider the
exposure dose as a parameter to adjust. Keep in mind that he surface of your
substrate may influence the optimum exposure dose. Resist on sputtered gold
needs more light compared to the same resist on bare silicon. The bake
condition you mentioned seems to be OK for a standard 1um thick positive
type photoresist.

Frank.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics