MEMSnet Home: MEMS-Talk: Al thermal evoporation
Al thermal evoporation
2005-04-02
RAY
2005-04-03
Yeswanth Rao
2005-04-04
li cai
2005-04-04
Andrew Xiang
2005-04-04
Joe Lonjin
Al thermal evoporation
Andrew Xiang
2005-04-04
I know faster the Al deposition rate, the better reflectivity for the
mirror.

You are saying better uniformity and adhesion if evaporation is slow. What
is the rate are you talking about?

Do the above 2 comments contradict with each other?

-Andrew

> You could use E-Beam Evaporation and may also try a slow rate of
> evaporation
> for better uniformity and adhesion. We are able to deposit very thick
> layers
> of aluminum (usually around 6 micron) by E-Beam Evaporation. Good Luck!

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.
The Branford Group