how to deposite low stress Si3N4
2005-04-12
Liu X.F.
2005-04-12
Eric Miller
2005-04-14
Shile
how to deposite low stress Si3N4
Liu X.F.
2005-04-12
Dear members of the MEMS community,

 I need deposite a layer of low stress Si3N4 on Si(100) substrate by LPCVD with
SiH4 and NH3 as precursors,but I wonder how to setup the condition such as
temperature,pressure,and the mass flow of SiH4 and NH3 respectively.

Any help will be appreciated.

thank you very much!

anodle
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation