MEMSnet Home: MEMS-Talk: Re: Anodic Bonding
Re: Anodic Bonding
2005-04-13
John Coppeta
Re: Anodic Bonding
John Coppeta
2005-04-13
I recently read an article describing a room temperature anodic bonding
process using an intermediate layer composed of a low melting temperature
glass. The article reference is:
Esashi, M., et. al. "Low-temperature Silicon-to-Silicon Anodic Bonding with
Intermediate Low Melting Point Glass", Sensors and Actuators, A21-A23
(1990), 931-934.

While the article is cited a few times, I have not found any additional
publications on the process.  Is anyone aware of additional research on this
process?
_________________________________
Jonathan Coppeta, Ph.D.
Process Development Manager
MicroChips Inc.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group