A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: is there anything else replacing SiO2 or Si3N4 for Sietch mask (KOH)?
is there anything else replacing SiO2 or Si3N4 for Sietch mask (KOH)?
2005-04-15
Joe Lonjin
2005-04-17
Nikhil Mehta
is there anything else replacing SiO2 or Si3N4 forSietch mask (KOH)?
2005-04-18
Shile
is there anything else replacing SiO2 or Si3N4 for Sietch mask (KOH)?
Nikhil Mehta
2005-04-17
yes... Brewer protex works great and we have used it.. to protect against KOH ..
it gets removed with acetone.. however if you have small dies and not the wafer
it did not work.. we used room temp PECVD process to grow hydrogenated DLC as
etch stop in that....
 case

hope that helps..

N

Joe Lonjin  wrote:
Brewer Science has a new material called protek which is specifically
for KOH/TMAH etching. Go to their web site, all the info is there.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
MEMStaff Inc.
Tanner EDA by Mentor Graphics