Marc,

The omnicoat stripper will have no effect on exposed and developed SU-8
- at that point, the SU-8 is pretty much immune to any solvent
chemistries. Basically, as long as the SU-8 processing has progressed
through the post-exposure bake (PEB) process, it will be unaffected.
However, the stripper for Omnicoat (remover PG) will also remove
unexposed SU-8, in effect becoming a developer solution. It will also
probably attack any exposed, but non-PEB SU-8 material.

Best Regards,
Chad Brubaker



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics