MEMSnet Home: MEMS-Talk: Anodic bonding oxidized Silicon wafers to Glass
Anodic bonding oxidized Silicon wafers to Glass
2005-04-19
Charles
2005-04-21
Tony Rogers
2005-04-20
Brubaker Chad
Anodic bonding oxidized Silicon wafers to Glass
Charles
2005-04-19
We have sucessfully bonded pyrex 7740 and borofloat glasses to bare
silicon wafer many times (so we have the equipment and some
understanding). We are now developing a process which requires attaching
pyrex 7740 glass to an oxidized silicon wafer.  The oxide will be 200nm
or so thick.  Does anyone have experience with this type of anodic
bonding? Is it possible? Any suggestions?

Thanks,
Charles Ellis....
Auburn University

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering