anybody having tried to anodically bond AF-45 glass wafers to Si wafers?
AF-45 is alkali-free, is it thus not suitable for anodic bonding? How does
it bond compared to Corning Pyrex 7740? I heard different opinions from
experts ...

Joachim Oberhammer, Ph.D.