A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Questions about DC-bias in dry etching
Questions about DC-bias in dry etching
2005-04-21
xiaodong wang
2005-04-22
William Lanford-Crick
2005-04-21
xiaodong wang
2005-04-22
Paolo Tassini
2005-04-21
[email protected]
2005-04-22
xiaodong wang
2005-04-22
xiaodong wang
Questions about DC-bias in dry etching
[email protected]
2005-04-21
Xiaodong,

How different are the sizes of the samples? (10%, 50%, etc) Also, what is the
size of your sample vs the carrier wafer and how are you holding them together?
If your DC bias is changing, I assume you are fixing your RF power, right?  The
DC bias depends on the RF power and the chemical reaction so, if the small
sample is the one with the 10V bias, it sounds like your sample size is small
enough that the reaction products for the small sample barely produce a bias.

Ramon Figueroa

----- Original Message -----
From: xiaodong wang 
Subject: [mems-talk] Questions about DC-bias in dry etching
> I have questions about DC-bias in dry etching.
>
> Conditions:
> I use the same recipe, size of carrier wafer and Therma plasma
> (dry etching machine),
> only slight difference may be the size of the samples (on the
> carrier wafer).
>
> Results:
> for example, the DC bias for the first sample is 90 V,  the bias
> for the second sample is 10 V
> sometime it is 0. Etching results are very different.
>
> My questions:
> what are the parameters affecting the DC bias?
> why are there so much difference of the bias in my etching
> condictions.
> Anyone had this kind of experience?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing