Michael D Martin
2005-04-22
BOE will definitely attack Ti. You might want to switch to a plasma oxide
etch.

-Mike Martin

>>> [email protected] 04/21/05 1:55 PM >>>
Hello folks,
 I am trying to etch away 1.6 micron thick thermal
oxide using 6:1 BOE. I have a 2 micron film of
Nickel-Titanium alloy beneath the oxide, and am
concerned whether the BOE will attack that film. Does
somehow have any experience about whether BOE attacks
Ni or Ti, and if so, what are typical etch rates?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.