2005-04-27
Steven McMaster
2005-04-27
Gary
2005-04-28
Steven McMaster
2005-04-28
Gary
Diffusion barrier for Ga into Au
Steven McMaster
2005-04-28
Gary,
Thanks for your mail. Do you have any more information on TiN, i.e. sheet
resistance, which thickness, grade of N, correct stochiometry etc?

Regards,
Steven.

-----Original Message-----
From: Gary
Subject: RE: [mems-talk] Diffusion barrier for Ga into Au

Try TiN, it is normally reactively sputtered and to be effective the
stochiometry must be "right on". Gary
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics