Ti etchant not attack glass
WILLIAMSON Fraser
2005-04-28
You can use a Ammonia and Hydrogen Peroxide solution.

Fraser
-----Message d'origine-----
De : Jauniskis, Linas [mailto:[email protected]]
Objet : RE: [mems-talk] Ti etchant not attack glass

Transene Inc has HF and non-HF versions of their Ti etch. Presumably the
non-HF version , which is HCl base, won't attack SiO2
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics