Re:spinning on thin layer of PDMS
2005-04-29
[email protected]
Re:spinning on thin layer of PDMS
[email protected]
2005-04-29
I got the same kind of results with RTV615 that Andrew did. If you're
spinning directly onto your part then you are ok, but if you need to
remove it, I'd suggest spinning on glass coated with acrylic enamel (spray
enamel or liquid). Then dunk the whole thing in ice water. Shrinks the
glass and expands the silicon - comes right off.

Any particular reason you don't use a photoresist like Shipley 5714? That
spins up to around 15 um thick or so. Don't remember the rpm off hand -
probably 2-3k.

Some tapes are also available around that thickness if you don't care to
much about exact placement.

Mike
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing