MEMSnet Home: MEMS-Talk: About pulsing substrate voltage biasing in dry etching
About pulsing substrate voltage biasing in dry etching
2005-05-09
xiaodong wang
About pulsing substrate voltage biasing in dry etching
xiaodong wang
2005-05-09
Anyone has experience in pulsing substrate voltage
biasing in DRIE?  What kind of frequency should chosed
for power supply? How to pulse the bias?

Thanks in advance.