MEMSnet Home: MEMS-Talk: non-mechanical polishing of PMMA
non-mechanical polishing of PMMA
2005-04-20
Mielnik, Michal
2005-04-20
Mac Daily
2005-05-12
Suk Sang Chang
non-mechanical polishing of PMMA
Suk Sang Chang
2005-05-12
I have been to make a PMMA microchannel with LIGA technique.
I think you can get a satisfactory results if you use it.

Thanks

-----Original Message-----
From: Mielnik, Michal
Subject: [mems-talk] non-mechanical polishing of PMMA

I am working with micromachined (milled) PMMA microchannels. The
dimensions are typically down to 50 microns.
However, the roughness of the surfaces after machining is somewhat high.
Does anyone have an idea on how I can polish these channels? (make
smooth walls). I cannot do it mechanically due to the dimensions. So;
Is it possible to simply flush them with e.g. some solvent like toulene
or dichloromethane to obtain smoother surfaces?
Any idea on flow rates and treatment times?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.