MEMSnet Home: MEMS-Talk: Initial Stress of SU-8
Initial Stress of SU-8
2005-05-12
yanli Wang
2005-05-12
Michael L
2005-05-12
Brubaker Chad
Initial Stress of SU-8
Brubaker Chad
2005-05-12
It is definitely tensile stress, as can be seen in the propagation of
cracks in the patterned film.

Best Regards,
Chad Brubaker

 -----Original Message-----
From: yanli Wang
Subject: [mems-talk] Initial Stress of SU-8

I would like to know the initial stress of SU-8. Is the SU-8 compressive
stress or tensile stress?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
Tanner EDA by Mentor Graphics