A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: metal oxidation at 200C
metal oxidation at 200C
2005-05-19
Tan, Chuan Seng
2005-05-19
vic kley
2005-05-19
[email protected]
How to take a cross section SEM pictures?
2005-05-24
[email protected]
2005-05-30
Duan
2005-06-01
Shay Kaplan
metal oxidation at 200C
[email protected]
2005-05-19
Chuan,
If you need no oxidation at all, gold or platinum are your choice  They
need an adhesion layer
You can use aluminum since the oxide formed is self limitting and very
thin W might grow thick oxides
Shay

Original Message:
-----------------
From: Tan, Chuan Seng
Subject: [mems-talk] metal oxidation at 200C

Does anyone know of any metal that can stand heating up to 200C in room
ambient without servere oxidation ? It is ok to have an outer layer of
oxide as long as the oxidation is self-limiting

Any comments about Al or W ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing