A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Through holes etching - aspect ratio > 20
Through holes etching - aspect ratio > 20
2005-05-22
Pradeep Dixit
2005-05-23
Brian Dick
Through holes etching - aspect ratio > 20
Pradeep Dixit
2005-05-22
Dear All,

Has any one achieved 15-20 microns "through holes" in 400-450 thick
wafer. Aspect ratio > 20 ?

Please let me know if any one has got success in it.
--
Thanks,
Pradeep Dixit