Dear All

After looking through the archive I could not find a answer to my
problem. I would like to remove 15 micron gold which has been plated
on the surface of GaAs without etching the GaAs. I tried KI + I2 + H2O
but this solution attacks GaAs. I would be thankful for you help.

Yours sincerely

Naser