MEMSnet Home: MEMS-Talk: ebeam Ni, crucible?
ebeam Ni, crucible?
2005-05-28
X.P. Zhu
ebeam Ni,crucible?
2005-05-28
Oray Orkun Cellek
2005-05-29
Pradeep Dixit
2005-05-29
Shay Kaplan
2005-05-28
Charles Ellis
2005-05-31
Joe Lonjin
ebeam Ni, crucible?
Pradeep Dixit
2005-05-29
You can use thick graphite crucible for Ni evaporation. We are using
it from long time.

On 5/28/05, X.P. Zhu  wrote:
> Dear members,
>   I am using E-beam to evaporate Ni. The crucible is
> made of tungsten. But it seemed that fused Ni could
> "eat" tungsten. I wonder whether they have formed some
> kind of alloys. Should I replace the tungsten crucible
> by other metals, such as molybdenum? Thank you very
> much.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Addison Engineering
The Branford Group