MEMSnet Home: MEMS-Talk: C4F8 clean
C4F8 clean
2005-05-31
sanky
2005-05-31
[email protected]
C4F8 clean
sanky
2005-05-31
Hello all,
I was wondering if anyone knew how to clean a RIE chamber after using C4F8
plasma.
My C4F8 processing conditions are about 400 W, 10mtorr, 20 sccm and the chamber
gap is 4 cm and diameter is 60 cm.
I use C4F8 for about half n hour. So i am wondering if a 1-1 C4F8 / O2 clean
time wud be enough....
Also i have a OES hooked up to the chamber, so i was wondering if monitoring the
emission between 200 to 600 nm would give me a
clean trace of the chamber.

Sanket Sant
Doctoral candidate
Plasma Science lab
University of texas at dallas.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation