PDMS bonding to glass
2005-06-01
[email protected]
2005-06-01
Lee Pang
2005-06-02
[email protected]
antireflection coating?
2005-06-03
[email protected]
2005-06-03
Robert Black
2005-06-07
John Maloney
PDMS bonding to glass
[email protected]
2005-06-02
Lee,

I can't tell you much more about the tool I used. It was simply called a
UV/ozone cleaner and I don't remember the brand. Looked like a large bread
box. Basically just a UV light and a tray. The UV generates the ozone. No
optical filters or anything like that. Basically (I'm theorizing) it just
breaks some of the surface chemical bonds with the ozone. The lamp puts
out a lot of heat though so going more than a minute or two tends to
plasticize the PDMS and then it won't bond at all.

Here's a link to something very much like what I used:
http://www.equiptechonline.com/subsection.cfm?sid=4&subID=92

Mike
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics