Sputtered silicon nitride film ech rate
2005-06-03
harshal rokade
2005-06-04
Jessica Gomez
Sputtered silicon nitride film ech rate
Jessica Gomez
2005-06-04
Hi Harshal,

Sputtered silicon nitride (and low temperature PECVD Nitride as well) do not
hold up well to HF.  You may want to consider LPCVD nitride which is much
more HF resistant. For example etch rates for our low stress lpcvd nitride
in 10:1 HF are around 6A per minute.

Best Regards,

Jessica
-----Original Message-----
From: harshal rokade [mailto:[email protected]]
Subject: [mems-talk] Sputtered silicon nitride film ech rate

I am trying to get silicon nitride film from sputtering which wont get ethed
in HF. My surrent films are getting etched in HF in 30 secs. in wich
parameters does etch rates depends??
and what are those?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
MEMStaff Inc.
Addison Engineering