Hoyin,
   We have a group doing the same thing here at the Univesity of Louisville.
One bit data that may be usefull for you: they found that wirebonding with
a ball bonder which uses an electrostatic discharge to form the ball would
frequently destroy thier devices.

-Mike Martin

>>> [email protected] 06/10/05 12:00 AM >>>

I would like to see if you can have experience in making measurement of a
CNT bridged electrode. Basically, I am trying to make a CNTFET. I found that
when I got a CNT bridged electrodes, it is extremely easy to be burnt. It
happens in CNT itself and the electrodes. I am guessing it is caused by
static charge in human body. I have already grounded myself while handling
the CNT bridged electrodes and taking IV measurement. The condition for the
IV measurement is in air and room temperature. Also, I found that the
current is extremely small which is ~1E-12 A. People always have current up
to couple nanoamps or more. I know that they may take the measurment under
vaccum. So, I would like to see whether you can share your experience with
me.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
University Wafer
MEMS Technology Review