Estimation of Mass using commercial thickness monitor.
2005-06-12
Sungjun Lee
Estimation of Mass using commercial thickness monitor.
Sungjun Lee
2005-06-12
Dear all,

I would like to use a thickness monitor (TM) to estimate the mass of unkown
 material's we evaporated.
(As you may know well, the density and Z ratio should be known to measure
 the thickness.)
The TM can detect the change of resonance frequency with a relationship
 between the mass and the stiffness.
Therefore, I think the mass change could be taken simply without measuring
 resonator's initial mass.
Could you please advice me about this work?
Thank you in advance.

Lee


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Addison Engineering
The Branford Group