On Sun, 12 Jun 2005 08:37:51 -0600 "li cai"  wrote:
> Deposit thin Ti first, then Au.  After that, do plating.
>

Krishna, As Li said , evaporating a thin Ti layer should work perfect in your
case. I have tried the same before and it worked for me. Au does not have a
very good adhesion to resist and you needa  Ti seed layer.

Sumant Sood
Belford Research
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
MEMStaff Inc.
The Branford Group