RE: cantilever bending problem ?
2005-06-15
Tom Rust
RE: cantilever bending problem ?
Tom Rust
2005-06-15
If you are using a wet release process, the cantilevers are almost
certainly sticking to the substrate due to wetting and stiction between
the cantilever and the substrate.
You need a much deeper thicker material under the cantilever, or try a
dry release process. But a 100u undercut will take a long time -
depending on what sacrificial material you are using.

--
Tom Rust
Nanochip Inc
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review