MEMSnet Home: MEMS-Talk: Mechanically machining thick [~4 mm] Silicon.
Mechanically machining thick [~4 mm] Silicon.
2005-06-15
Alderete, Michael
2005-06-16
Martin Heller
2005-06-16
Shivalik Bakshi
2005-06-16
Paul Hines
2005-06-16
Shay Kaplan
Mechanically machining thick [~4 mm] Silicon.
Martin Heller
2005-06-16
Dear Michael,
take a look at http://www.kern-microtechnic.com/2-Test-Silicon.html
We've got one Kern HSPC at my old university and it's really an
awesome machine for using "classical" methods at the micro scale.

Regards,

Martin

-------------------------------------------
Martin Heller
Fraunhofer Institute for Silicon Technology

Alderete, Michael wrote:
> Does anyone have experience with the mechanical machining of thick
> [approximately 4 mm thick] Silicon?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer