unexpected etching pattern
2005-06-17
xiaoyu
2005-06-17
Shile
unexpected etching pattern
xiaoyu
2005-06-17
I am testing a capacitive RF etching chamber. And when used
30sccm argon gas to sputter with a power of 100W, my wafers
(coated fairly with ~70nm fairly uniform SiO2) came out with
a bizzare pattern. The 3d view of the etched samples resemble
a hill, with its edges etched the most, and the center the
least. This was without using any photoresist or mask. I
would greatly appreciate any plausible explainations.

Xiaoyu

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review