RE: Charge effects in electrostatic actuators
2005-06-20
Jia, Nancy
Through wafer etching with KOH - mask
2005-06-21
Simon Garcia
2005-06-21
Hongjun-ECE
2005-06-21
Shay Kaplan
RE: Charge effects in electrostatic actuators
Shay Kaplan
2005-06-21
Nancy,
If you oxide is good, you will end up having trapped charge, it's a matter
of time and quantity.
The way to avoid it is to supply some leakage mechanism -i.e. high value
resistor in series.
shay

-----Original Message-----
From: Jia, Nancy
Subject: [mems-talk] RE: Charge effects in electrostatic actuators

This is based on a typical MEMS Surface Micromachining Process.   It is
like a parallel capacitor with a fixed polysilicon electrode at the bottom
of the device and a movable doped polysilicon membrane on the top that is
grounded.  There is a thermal oxide or nitride deposited on the fixed
polysilicon to prevent electrical shorting between the two
electrodes.   Hope this give you enough details to answer my original
questions.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.