MEMSnet Home: MEMS-Talk: Preparation of NiTinol sample for SEM
Preparation of NiTinol sample for SEM
1998-05-01
Mizar Pai Shivananda
Preparation of NiTinol sample for SEM
Mizar Pai Shivananda
1998-05-01
Hello..

I am interested in preparing a sample of NiTi (equiatomic) for viewing under
the SEM. I will be using an aqueous solution of HF and Nitric Acid for etching
the sample..But I am not sure whether I can polish the sample mechanically and
still not have a change in the microstructure.

Thanks,,

                Sincerely:
                        Mizar Shivananda Pai.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review