Does O2 plasma attack teflon?
2005-06-22
X.P. Zhu
2005-06-22
Zhiliang Wan
2005-06-22
[email protected]
Does O2 plasma attack teflon?
Zhiliang Wan
2005-06-22
Hi, Zhu,

Yes, O2 plasma will attach Teflon. I'm using O2 plasma to pattern Teflon
film and it works very well.

Zhiliang

At 08:30 PM 6/21/2005, you wrote:
>Dear all,
>We use a teflon holder to hold wafers. I wonder
>whether it can be etched during the wafer cleaning
>process by using O2 plasma. Can anybody tell me?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
Nano-Master, Inc.