microlens
Jason Milne
2005-06-30
Hi Mohammed

I've had success decreasing the contact angle by spinning on a very thin
film of the same resist, and baking this layer hard (not too sure about
your resist, but bake it long enough so that it doesn't develop). Then
use your usual process for making the microlenses.

Jason Milne



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of mohammed ashraf
Sent: Monday, 27 June 2005 7:07 PM
To: [email protected]
Subject: [mems-talk] microlens

Hi all
I need to decrease the contact angle while reflowing microlenses.Can
somebody suggest a practical way of increasing the hydrophillicity of
Si-substrate wrt PR(AZ9260cp).
Regards
Mohammed Ashraf

_________________________________________________________________
44 Million Items on Sale.What Are you Looking for?
http://adfarm.mediaplex.com/ad/ck/4686-26272-10936-377?ck=44MilItems
Find it
on eBay.in!

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.
MEMS Technology Review